Skip to main content
. 2018 Jul 11;11(7):1192. doi: 10.3390/ma11071192

Figure 2.

Figure 2

Macrostructure of the plate penetration run performed using a laser beam power of 7 kW, the outlined fusion line, and the outline of the penetration run plotted on the schematic diagram of the T-joint.