Figure 6.

Figure 6

SEM enlargements taken at 500× (left) and 2,000× (right) of the TM (a, b) and TSV (c, d) surfaces, respectively. Note the irregular faceted tantalum surface texture (top row) compared to the relatively uniform microtextured titanium surface (bottom row) caused by the CVD and grit‐blasting surface preparation methods, respectively