Physicochemical characterization of NPs (n ≥ 3)

PLGA-NPs SPIO-NPs PTX-NPs PTX/SPIO-NPs
Size (nm) 215 ± 4 225 ± 12 203 ± 4 250 ± 20
PDI 0.07 0.09 0.07 0.11
Zeta potential (mV) −8.6 ± 1 −13 ± 5 −21 ± 3 −18 ± 5
Drug encapsulation efficiency (%) NA NA 31 ± 2 30 ± 6
Drug loading (%) NA NA 0.85 ± 0.3 0.87 ± 0.2
Iron loading (%) NA 4 ± 1 NA 3 ± 1

Notes: physicochemical characterization of PLGA based PEGylated NPs (PLGA-NPs) loaded with either SPIO (SPIO-NPs), PTX (PTX-NPs), PTX and SPIO (PTX/SPIO-NPs).

Abbreviations: NA, not applicable; NPs, nanoparticles; PDI, polydispersity index; PLGA, poly(lactic-co-glycolic acid); PS80, polysorbate 80; PTX, paclitaxel; SPIO, super paramagnetic iron oxide.