Fig. 8.

Fig. 8

Mass corrosion index of the external (a), middle (b) and bottom (c) layer of the metallic multilayer material at different diameters (d, mm) of an artificial lens, diameter of an artificial pitting of 1 mm and exposure time of 720 h (curve 1) and 2,208 h (curve 2).