Skip to main content
. 2018 Jun 4;5(8):1800065. doi: 10.1002/advs.201800065

Figure 7.

Figure 7

Degradation degree of cationic polymers under different test conditions: a) in 2 m KOH D2O solution at 80 °C for 24 and 96 h, respectively, b) in 2 m KOH mixed solution (VD2O/VCD3OD=1:1) at 80 °C for 24 and 96 h, respectively, c) in 2 m KOH CD3OD solution at 80 °C for 24 and 96 h, respectively.