Skip to main content
. 2018 Aug 5;2018:9415965. doi: 10.1155/2018/9415965

Figure 2.

Figure 2

Effect of H2O2 concentration on degradation of UPP. The reaction temperature was 80°C and pH 4 was used. Different H2O2 concentrations varying from 0.15% to 4.5% were tested.