Table 2.

Properties of NMs’ deposits and photoabsorption properties of metal-modified titania samples.

Titania NM Sample color λmaxa
(nm)
Predominant crystalline formb Crystal size of zero-valent metalb /nm Crystal size of metal oxideb /nm
OAP Au violet 544 Au 5.7
DAP violet 563 Au 14.7
OAP Ag l. brown-violet 415 Ag2O 7.5 14.6 (Ag2O)
DAP violet-blue 554 Ag 37.1 64.2 (Ag2O)
OAP Cu l. green 789 CuO 8.1 5.7 (CuO)
DAP l. grey-violet 676 CuO 44.9 67.5 (CuO)
a

maximum extinction from DRS.

b

estimated from XRD.