Figure 1.
Conventional silanization procedure (left) and novel two-step silanization protocol (right): First the reaction mixture is acidified with HCl to pre-hydrolyze the alkoxysilane, then NaOH is added to induce condensation in this homogeneous system. Following this protocol, azido, vinyl, and thiol groups were introduced onto never-driedcellulose surfaces.