Figure 11.

Figure 11

Figure 11

A typical weld pool behavior during the formation of lack of fusion in MPAW of edge weld. (a) t0; (b) t0 + 80 ms; (c) t0 + 160 ms; (d) t0 + 240 ms; (e) t0 + 320 ms; (f) t0 + 400 ms; (g) t0 + 480 ms; and, (h) t0 + 560 ms.