Skip to main content
. 2018 Jul 27;11(8):1298. doi: 10.3390/ma11081298

Table 6.

Flammability of SR/POSS composites.

Sample TTI
(s) ± 5
THR
(MJ/m2) ± 1
HRR
(Kw/m2) ± 2
HRRMAX
(kW/m2) ± 2
EHC
(MJ/kg) ± 2
EHCMAX
(MJ/kg) ± 1
MLR
(g·m−2·s−1) ± 0.01
SR 93 21.6 73.62 124.73 37.22 79.82 0.064
SR/AM3 91 18.1 59.81 102.67 38.88 77.80 0.049
SR/HA3 80 20.3 73.59 120.26 36.50 61.50 0.051
SR/OL3 85 19.3 62.49 105.50 34.41 76.49 0.061
SR/AM6 114 14.1 52.81 88.72 30.49 61.44 0.057
SR/HA6 106 20.7 60.58 106.45 38.1 77.42 0.050
SR/OL6 99 13.5 38.72 66.10 31.72 78.05 0.036

TTI—time to ignition; THR—total heat release; HRR—heat release rate; HRRMAX—maximal heat release rate; EHC—effective combustion heat; EHCMAX—maximal effective combustion heat; MLR—mass loss rate.