Skip to main content
. 2018 Jul 27;11(8):1296. doi: 10.3390/ma11081296

Figure 8.

Figure 8

Relation between Na2O concentration and the strength of AAS mortar after exposure to high temperature range: (a) From laboratory temperature to 200 °C; and, (b) From 800 to 1000 °C.