Skip to main content
. 2018 Aug 8;11(8):1383. doi: 10.3390/ma11081383

Figure 2.

Figure 2

Percentage of undegraded sample (1 − D)%, at 150 °C as a function of heating time (t) for PE (sample 4 □), PS (sample 5 △), PC (sample 6 ○), and PMMA (sample 7 σ) after 200 days of degradation.