Optimal processing parameter values to be used for PCL scaffold printing.

Title Parameters Optimal Values
Manufacturing parameters Extruder temperature 85 °C
Bed temperature 35 °C
Deposition velocity 10 mm/s
Layer height 0.3 mm
Design parameters Filament diameter 0.3 mm
Distance between filaments 0.7 mm
Deposition angle 60° (MCF-7 breast cancer cells)