Skip to main content
. 2018 Aug 14;11(8):1426. doi: 10.3390/ma11081426

Figure 8.

Figure 8

(A) Growth of the amount of Bi deposited in one minute on Ag electrode in function of the deposition potential; (B) amount of deposited Bi with a potential fixed at −0.45 V depending on the deposition time.