Skip to main content
. 2018 Jul 31;11(8):1326. doi: 10.3390/ma11081326

Table 5.

Thermal data of the poly (tetramethylene oxide) (PTMO) melting peak from DSC curves for ‘as prepared’ films (T0 samples) and photo-exposed Pebax®2533 films (6 h).

Preparation Method Casting Solvent Hm (J g−1) Xc (wt.%)
T0 6 h T0 6 h
Solution casting ethanol 32.8 31.2 23.4 22.3
i-propanol 38.3 30.1 27.3 21.4
HFIP 35.8 22.5 25.5 16.0
1-butanol 47.0 30.2 33.5 21.5
Hot press - 36.2 29.4 25.8 21.0