. 2018 Aug 16;11(8):1451. doi: 10.3390/ma11081451

Table 1.

Attached nisin content (Bradford assay from electrophoresis) and nitrogen content (TN) on the PVA surface (PVA films were stored at 25 °C for 3 months, relative humidity 54%). Nisin content on untreated PVA films was not measurable, and SD was higher than calculated value.

PVA/Nisin-Buffer Crosslinking Degree (%) Nisin Content (µg/mm2) TN (µg/mm2)
0 1.8 ± 0.5 0.7
5 3.6 ± 1.5 4.3
10 31.4 ± 1.5 13.2
20 28.2 ± 1.5 9.7
40 19.3 ± 1.3 6.8