Skip to main content
. 2018 Sep 7;8:13407. doi: 10.1038/s41598-018-31716-8

Table 1.

Mechanical properties of SLS parts.

laser Power (W) Tensile strength (MPa) Bending strength (MPa) Elongation at break (%)
PA12 powder 6 34 ± 2.6 38 ± 4.2 26.8 ± 3.1
10 42 ± 3.1 44 ± 1.9 20 ± 2.5
Ni/PA12 composite powder 6 21 ± 2.1 36 ± 2.5 21.1 ± 1.8
10 50 ± 1.8 60 ± 3.5 10 ± 2.1