Characterization of an ss-DSSC/ALD/IrOx electrode as a photoanode. (A) Measured (lines) and calculated (squares) linear sweep voltammetric curves of the ss-DSSC/ALD/IrOx electrode. Scan rate: 20 mV/s. (B) Three-electrode photocurrent measurement at an applied bias of 0.62 V vs. Ag/AgCl. Light source: 100-mW/cm2 xenon lamp with a 410-nm long-pass filter and an AM1.5 filter.