Figure 4.
Temperature-Driven Self-Assembly of PMPC-PDPA Copolymer at Different Molecular Weight
(A–C) Turbidity measurement using UV/Vis absorbance at 400 nm of PMPC25-PDPA72, PMPC12-PDPA35, and PMPC6-PDPA12 solution during heating (red curves) and cooling (blue curves) starting from 5°C to 60°C; a photograph of the cuvette before and after heating is shown (A). TEM images of PMPC25-PDPA72, PMPC12-PDPA35, and PMPC6-PDPA12 structures formed during heating and after cooling. Scale bar, 200 nm (B). Micro-differential scanning calorimetry of PMPC25-PDPA72, PMPC12-PDPA35, and PMPC6-PDPA12 dispersion showing the heat exchange during heating and cooling (C).