Skip to main content
. 2018 Sep 21;8:14170. doi: 10.1038/s41598-018-32590-0

Figure 4.

Figure 4

(a) Measured normalized sheet resistance variation (ΔRs/Rs0 = (Rs(bent) − Rs0(unbent))/Rs0(unbent)) of PVB/AgNWs, ITO (tITO = 130 nm), and IZO (tIZO = 200 nm) electrodes on a PET substrate (tPET = 200 µm) as a function of bending radius. (b) Sheet resistance change of the PVB/AgNWs samples with and without IPL exposure, PET/IZO, and PET/ITO electrodes as a function of number of bending cycles. (c) Sheet resistance change of the PVB/AgNWs and Glass/AgNWs electrodes as a function of number of tape tests.