Susceptibility of a 2% w/v PEO solutions. Almost an 80% drop in viscosity was observed from at (A) ambient room temperature to (B) 95°C. (C) A complete precipitation was observed in ethanol. (D) The aqueous polymer (A) was easily syringeable at room temperature