Skip to main content
. Author manuscript; available in PMC: 2019 Sep 25.
Published in final edited form as: ACS Nano. 2018 Sep 14;12(9):9342–9354. doi: 10.1021/acsnano.8b04348

Figure 3. TEM characterization of.

Figure 3.

AuNS@PNM. (a) TEM image of DDT-capped, PMAO-g-PEGMA stabilized AuNSs. (b,c) TEM images showing mixture of coreless PNM nanogels AuNS@PNM with flower-like architecture at (b) 16,500× and (c) 43,000×. All samples were stained with 2% phosphotungstic acid (pH 7.0).