Characterization summary of 40:60 CDP146 ASDs produced by spray-drying (100 mg).

ASD Composition Yield Miscibility/Solid State
Polymer DL (w/w) Yield (%) Tg (°C) Tm (°C) XRPD Pattern/PLM
HPMCP HP50 40% 68.1 113.5 - A
HPMCAS-LF 40% 70.9 102.5 - A
Eudragit L100 40% 71.8 163.4 - A
Eudragit L100-55 40% 71.7 120.9 - A

A: amorphous sample characterized by the presence of a large halo in XRPD and the absence of birefringence under PLM observations.