Skip to main content
. Author manuscript; available in PMC: 2018 Sep 28.
Published in final edited form as: J Biomed Mater Res A. 2018 Apr 30;106(8):2213–2228. doi: 10.1002/jbm.a.36428

FIGURE 4.

FIGURE 4.

(a) Cyclic water uptake; (b) Swelling kinetics; and (c) Biodegradation degree of bioscaffolds up to four weeks; (d) SEM images of polydopamine coated-cryogel bioscaffold before and (e) after hydration-dehydration process. Significant differences: *p < 0.05, difference between uncoated- and polydopamine coated-cryogel bioscaffolds. (Unpaired student’s t test).