Fig. 5.

Fig. 5

a) Young's modulus, b) ultimate tensile stress and c) ultimate tensile strain of polymer films (80% polydimethylsiloxane [PDMS]), with and without nitric oxide (NO) exposure, after the incubation in phosphate-buffered saline (PBS) for 15 days.