Skip to main content
. 2018 Sep 5;11(9):1627. doi: 10.3390/ma11091627

Figure 4.

Figure 4

XRD pattern of as-prepared WNRAs film at 180 °C for 4 h with RMo/W of 1:40. FTO—fluorine doped tin oxide.