Skip to main content
. 2018 Sep 7;11(9):1654. doi: 10.3390/ma11091654

Table 5.

Average particle/cluster hydrodynamic diameter before and after thermally induced aggregation in the temperature range from 25 °C to Tonset1, measured and calculated for dispersions with 1 g L−1 concentration of polymer. The DH before and after are different with a significance value of 95%.

Sample DH,before  DH,after 
FeOx-5 19.7 ± 1.0 23.4 ± 0.7
FeOx-7 21.4 ± 0.7 25.5 ± 0.5
FeOx-10 20.0 ± 0.3 23.1 ± 0.6
FeOx-21 30.5 ± 0.4 33.9 ± 0.4