Skip to main content
. 2018 Sep 1;11(9):1573. doi: 10.3390/ma11091573

Figure 5.

Figure 5

Computed micro-tomography image of the MIM proceed porous titanium sample sintered at 1250 °C: (a) 3D view of the sample, (b) side view and (c) top view.