Skip to main content
. 2018 Sep 7;11(9):1643. doi: 10.3390/ma11091643

Figure 9.

Figure 9

Cutting temperature distribution of chip with SCT1 at speed of 100 m/min in dry cutting hardened steels (ap = 0.2 mm, f = 0.1 mm/r).