Skip to main content
. 2018 Sep 7;11(9):1643. doi: 10.3390/ma11091643

Figure 10.

Figure 10

Cutting temperature with SCT1 and SCT2 in dry cutting of hardened steel at different cutting speeds (ap = 0.2 mm, f = 0.1 mm/r, cutting time 5 min).