Skip to main content
. 2018 Sep 4;11(9):1603. doi: 10.3390/ma11091603

Figure 10.

Figure 10

Microstructural feature of the Ti6Al4V30Zr alloy after beta annealing at 1050 °C: (a) bright field (BF) image showing α″ laths; (b) SAD (selected area electron diffraction) pattern with [113] β zone axis; (c) HAADF-STEM images; (d) The EDS mapping of Zr, V, Al, and Ti atoms.