Microstructural feature of the Ti6Al4V30Zr alloy after aging at 600 °C: (a) bright field (BF) image; (b) SAD pattern with [111] β zone axis; (c,d) HAADF-STEM images showing α phase; (e) the EDS mapping of Zr, V, Al, and Ti atoms; (f) the composition profiles along the arrows shown in (d).