Skip to main content
. 2018 Sep 4;11(9):1603. doi: 10.3390/ma11091603

Figure 14.

Figure 14

SEM, backscattered electron images of the Ti6Al4V30Zr alloy after solution treated at 820 °C and aged at different temperatures: (a) 500 °C; (b) 550 °C; (c) 600 °C; (d) 650 °C.