Figure 3.

Figure 3

(a) Photo of the LVO film formed on a glass substrate by AD. (b) and (c) are SEM images for the surface and fractured cross-section of the LVO film on a glass substrate. XRD patterns for the LVO film formed on a glass substrate by AD and LVO powder are compared in (d).