. 2018 Sep 11;11(9):1685. doi: 10.3390/ma11091685

Figure 6.

Figure 6

XRD patterns of (a) Bi1.8Zr0.2O3.1 after heat treatment at different temperatures and Bi2−xZrxO3+x/2 (x = 0.2 to 1.0, 0.2 each) after heat treated at (b) 500 and (c) 750 °C.