Skip to main content
. 2018 Sep 11;11(9):1685. doi: 10.3390/ma11091685

Figure 9.

Figure 9

TEM images and SAED patterns of (ac) Bi1.8Zr0.2O3.1 and (df) Bi1.0Zr1.0O3.5 powders after heat treatment at 500 °C.