Skip to main content
. 2018 Sep 17;18(9):3136. doi: 10.3390/s18093136

Figure 12.

Figure 12

Performance parameters calculated by varying silver layer thickness d1 from 15 nm to 50 nm and gold thickness d2 of 15 nm (solid blue curve), 20 nm (solid red curve), 25 nm (solid yellow curve) and 30 nm (solid purple curve) when the incident wavelength λ was fixed at 632.8 nm and the applied potential ψ0 of 0 V at (a) minimum Rp; (b) FWHM. (c) Sensitivity calculated by comparing the plasmonic wave vector positions of applied potentials ψ0 of 0 V and 0.2 V and (d) FoM calculated from Figure 12b,c.