Notes: The cytotoxicity of MSNs and Ag-MSNs against (A) HaCaT cells and (B) NIH-3T3 cells at different levels of concentration after 24 hours. (C) Cumulative degradation profile of MSNs and Ag-MSNs under 10 mM GSH-containing SBF for 96 hours. These data represent three separate experiments and are presented as mean values±SD. *P<0.05 vs control group. TEM images of (D) MSNs and (E) Ag-MSNs after 48 hours of incubation in SBF containing 10 mM GSH; the scale bars represent 50 nm.