. 2018 Aug 1;10(8):e821–e830. doi: 10.4317/jced.54749

Figure 5.

Figure 5

(A) Bar chart representing the comparison of flexural strength, and (B) line chart representing the comparison of Weibull survival probability of flexural strength for translucency monolithic zirconia, sintered at decreasing (SD), regular (SR), and increasing (SI) sintering temperature, with shortening (HS), regular (HR), and prolonged (HP) sintered-holding time.