Skip to main content
. 2018 Aug 1;10(8):e821–e830. doi: 10.4317/jced.54749

Figure 6.

Figure 6

SEM photomicrographs indicated grain size and grain distribution of translucency monolithic zirconia, sintered at decreasing (A, B, C), regular (D, E, F), and increasing (G, H, I) sintering temperature, with shortening (A, D, G), regular (B, E, H), and prolonged (C, F, I) sintered-holding time at X30K magnification.