Table 1. Mean, standard deviation (SD), 95% confidential interval (CI), Weibull modulus (m), characteristic strength (σo), percentage of grain size distribution (%), and relative phase content (wt.%) for flexural strength (MPa) of translucency monolithic zirconia, sintered at decreasing (SD), regular (SR), and increasing (SI) sintering temperature, with shortening (HS), regular (HR), and prolonged (HP) sintered-holding time.