Representative optical micrographs (scale bar=20 μm) of the coating/metal interface in UV‐irradiated (two weeks exposure) bronze disks covered with a) HAVOH‐MBT and b) HAVOH‐LDH/MBT coatings before and after accelerated corrosion treatments of different duration. c) Percentage of corroded surface after accelerated corrosion treatment.