Fig. 5. (a) TEM of UiO-66 nanoparticles before aptamer conjugation in DMF. (b) TEM of HfMOF nanoparticles after phosphate-terminal aptamer conjugation in water. (c) TEM of UiO-66 nanoparticles after phosphate-terminal aptamer conjugation in water. (d) Powder X-ray diffraction of UiO-66 nanoparticles before (black) and after phosphate-terminal aptamer conjugation (red). Scale bar: 200 nm.