Figure 3.

Figure 3

Measurement rate of breakdown of PVA/chitosan scaffolds. Dry weight ratio or degradation behaviour (%) of PVA and chitosan/PVA hydrogels was measured using PBS at different time points. Graphical data are presented as mean (n = 3) ± standard deviation of three independent experiments