. 2018 Oct 12;4(10):eaat7629. doi: 10.1126/sciadv.aat7629

Fig. 2. Comparison of thermophysical properties of elastomers prepared using polyrotaxane cross-linking agent and general cross-linking agent.

Fig. 2

(A) DSC results of the MEO2MA elastomers prepared with HPR-C and EGDMA as cross-linkers. (B) TGA of the MEO2MA elastomers prepared with HPR-C and EGDMA as cross-linkers. (C) Temperature dependence of the storage modulus, loss elastic modulus, and tan δ obtained from the dynamic viscoelasticity measurements of the MEO2MA elastomers prepared with HPR-C and EGDMA as cross-linkers.