Skip to main content
. 2018 Oct 12;4(10):eaat7629. doi: 10.1126/sciadv.aat7629

Fig. 4. Mechanical properties of polyrotaxane cross-linked elastomers at various polyrotaxane concentrations.

Fig. 4

(A) Results of the uniaxial tensile tests and tear tests of the MEO2MA elastomers prepared with different amounts of HPR-C as a cross-linker. (B) Temperature dependence of the storage modulus of the MEO2MA elastomers prepared with different amounts of HPR-C or with EGDMA. (C) Temperature dependence of the loss modulus of the MEO2MA elastomers prepared with different amounts of HPR-C or with EGDMA. (D) Temperature dependence of tan δ of the MEO2MA elastomers prepared with different amounts of HPR-C or with EGDMA.