Machining conditions for EMM experiments.

Machining Conditions Parameter
Applied Voltage (V) 3.5–5.5
Pulse on Time (ns) 60–150
Pulse Period (μs) 1
Electrode Diameter (μm) 3–20
Workpiece Material Super alloy (GH3030)
Electrolyte 0.2M H2SO4 solution
Mill Layer Thickness (μm) electrode diameter
Feed Rate (μm/s) 0.2–1