Surface morphology and cross observations of Nb2O5 thin film deposited at (a) room temperature (RT), (b) 300 °C, and (c) 400 °C, respectively. (d) Cross-section observation of Nb2O5 thin films, the deposition temperature was 200 °C and the O2 ratio was 10%, respectively.