Skip to main content
. 2017 Feb 21;9(3):33. doi: 10.1007/s40820-017-0136-6

Fig. 2.

Fig. 2

SnO2 nanowires grown on FTO at a 520 °C, b 620 °C, c 670 °C with no catalyst, and d from additional solution of FTO spin-coated onto the original thin film grown at 570 °C