Fig. 3.

Fig. 3

In situ XRD measurements of graphite during charging and discharging. Top: galvanostatic voltage profile measured at a current density of 10 mA g−1 for the first two cycles. Bottom: XRD patterns of graphite during cycling. The white horizontal dashed lines correspond to computed positions for different stages (shown in Fig. 2a)